Surface analysis of Rh/CdS
Isaac Bernard Rufus
,
Balasubramanian Viswanathan
,
Joseph C. Kuriacose
Published in Kluwer Academic Publishers
1995
DOI:
10.1007/BF02565271
Volume: 14
Issue: 1
Pages: 15 - 18
Abstract
[No abstract available]
View more info for "
Surface analysis of Rh/CdS
"
Request full-text
Cite
Content may be subject to copyright.
Citations (1)
References (19)
Related Papers (3)
Journal Details
Concepts (19)
Related Papers (3)
Articles
Davydov split PL emission and EPR correlation in β-mns layered cds nanorods
2009
Articles
Optical absorption and photoluminescence studies on CdS quantum dots in Nafion
2002 | AIP
Download
PDF
Publisher Copy
Articles
Syntheses and structural characterization of vanado-tellurites and vanadyl-selenites: SrVTeO5(OH), Cd2V2Te2O11, Ca3VSe4O13·H2O and Ba2VSe3O10
2017 | Academic Press Inc.
About the journal
Journal
Journal of Materials Science Letters
Publisher
Kluwer Academic Publishers
ISSN
02618028
Open Access
No
Concepts (19)
Cadmium compounds
Characterization
Electrochemistry
Interfaces (materials)
Oxidation
Oxides
Reduction
Rhodium
Scanning electron microscopy
Solutions
Sputtering
X ray photoelectron spectroscopy
ARGON ION SPUTTERING
OXIDE SULFIDE SOLUTION
Photocatalyst
PHOTODEPOSITION
Photoelectrochemical
Surface analysis
Surface treatment
Get all the updates for this publication
Follow